If you’ve ever ordered custom glass powder for a coating, ceramic glaze, or filtration project, you know that particle size distribution (PSD) isn’t just a “nice-to-have” detail—it’s the difference between a smooth, even finish and a lumpy, inconsistent mess. As a glass powder supplier, I get more questions about how we verify our PSD than almost any other part of our production process. Clients will say, “The last batch I got from another vendor was all wrong, and it ruined my entire run.” That’s why I want to break down exactly how we measure PSD, why each step matters, and what red flags to look for when you’re checking powder quality for your next project. Glass Powder
![]()
First, let’s cut through the jargon a little. PSD is the range of particle sizes in a powder sample, usually reported as a curve or percentage of material by volume (or sometimes number) that falls into specific size ranges. For glass powder, which we produce in a range from 10 nanometers for high-performance optical coatings up to 100 micrometers for general abrasives, getting this right is non-negotiable. If you’re making a UV-cured coating, too many oversized particles will scratch the surface; if you’re adding glass powder to a ceramic glaze, a wide PSD might lead to uneven melting and craze lines. So how do we measure this accurately? We rely on two primary methods in our lab, depending on the powder’s size range, and we run quality checks at every step of production—from raw glass cullet testing to the final packaged batch.
Let’s start with the method we use for most of our industrial-grade glass powder, which falls between 1 micrometer and 100 micrometers: laser diffraction. This is the workhorse of powder PSD testing, and it’s not just a random lab trick—it’s based on solid physics. When a laser beam hits a particle, it scatters at an angle that’s directly proportional to the particle’s size: smaller particles scatter light at wider angles, larger particles scatter at narrower angles. Our lab uses a Malvern Mastersizer, a benchtop instrument that takes thousands of readings per second, converts the scattered light data into a PSD curve, and gives us numbers like D10, D50, and D90—terms every powder buyer should know by heart.
Wait, let’s explain those D values because if a supplier only tells you “10 micron glass powder,” they’re probably leaving out critical context. D10 is the size where 10% of the powder by volume is smaller than that number. D50 is the median size—half the powder is smaller, half is larger. D90 is the size where 90% is smaller, so only 10% is larger. For example, if we say our standard 15 micron glass powder has a D50 of 14.8 microns, D10 of 8.2 microns, and D90 of 22.1 microns, that tells you the range and how tightly the sizes are clustered. A tight distribution (small gap between D10 and D90) means consistent particles, which is what you want for most applications. A wide distribution might be cheaper, but it will lead to uneven performance.
When we run a laser diffraction test, we don’t just pour a scoop of powder into the machine and hit start—sample preparation is everything here, especially with glass powder, which can be static-prone. Static electricity makes particles clump together, so we have to avoid that at all costs. First, we take a representative sample, not just the top of a bulk bag (the fines settle at the bottom, coarse particles at the top, so that’s a biased sample). We use a riffle splitter to divide the bulk material into equal, representative subsamples—this is the same tool we train our production staff to use when splitting samples for customer orders. Then, we disperse the powder properly: for dry powder, we use compressed air to gently agitate the particles and break up clumps, or for very fine powder (under 10 microns), we use a liquid dispersion medium, usually ethanol or deionized water with a small dispersant, to eliminate static. We test each sample three times to make sure the readings are consistent—if the D50 varies more than 0.5 microns between runs, we discard that sample and start over.
For our finer grades of glass powder, under 1 micrometer, laser diffraction is still useful, but we pair it with dynamic light scattering (DLS) because it’s more accurate for nanoscale particles. DLS works by measuring the fluctuations in scattered light as small particles move randomly (Brownian motion) in a liquid. The speed of their movement tells us their size: smaller particles move faster, so they create faster fluctuations in the light signal. This method is perfect for our 10 nm to 1000 nm glass powder used in optical films and precision abrasives. But here too, sample prep is critical: nanoscale glass particles are prone to agglomeration, so we use a high-pressure sonicator to break up clusters before running the test, and we measure the zeta potential of the dispersion to make sure the particles are charged enough to stay separate.
We also use one more method for quality control, especially for our coarser grades (over 100 micrometers) that are used in filtration media and sandblasting: sieve analysis. This is the oldest, most straightforward PSD testing method, and it’s still reliable for larger particles. We stack a series of woven metal sieves with progressively smaller mesh sizes on top of each other, weigh a pre-dried sample of glass powder, pour it into the top sieve, and shake the stack for a set amount of time (usually 15 minutes with a mechanical shaker) so particles fall through the meshes until they get stuck on the sieve that’s too small for them. Then we weigh the powder on each sieve, and calculate the percentage of total powder that falls into each size range. For example, if a 200-micron sieve has 5% of the powder left on it, that means 95% of the powder is smaller than 200 microns. We love sieve analysis because it’s easy to verify for clients—if you ever need to check a batch yourself, you can borrow or buy a sieve stack and run the test on-site, which is a huge plus for many of our industrial clients.
Now, let’s talk about what can go wrong here, because that’s the part most suppliers don’t tell you. A bad PSD test result doesn’t always mean bad powder—it could mean a bad test. We’ve seen this happen with clients who run their own in-house tests and get way different numbers than our lab. The most common mistakes? Using an unrepresentative sample (digging from the top of a bulk tote), not breaking up clumps for fine powder, or using a sample that’s too small. For example, if you take a 10-gram sample of a 5000-gram batch of powder, you might accidentally pick up a lot of fines or a lot of coarse particles, leading to a skewed PSD. That’s why we always include a copy of our lab’s test report with every order, along with instructions on how to take a sample to verify the result on your end.
Another thing that affects PSD, and that many people don’t consider, is how the glass powder is stored and handled after it leaves our facility. Glass powder is hard, but it’s also brittle. If you jostle or agitate it excessively during shipping, coarse particles can break down into smaller ones, or fines can clump together. That’s why we package all our glass powder in airtight, plastic-lined drums with foam padding to prevent shifting, and we recommend storing it in a cool, dry place away from excessive vibration. We always tell clients: if you run a test a week after receiving the batch and the PSD is different, check how you stored it first—chances are it wasn’t our product.
As a supplier, this PSD testing isn’t just about checking boxes for quality control. It’s about making sure the product you get works for your specific application. For example, a client last year was making self-leveling epoxy flooring, and they were having issues with uneven texture and surface scratchiness. They ordered a batch of 20-micron glass powder that another supplier said met their specs, but when they ran laser diffraction, the D90 was 45 microns—way higher than the 25 microns they needed. We tested a sample of that same powder (they sent us a small portion) and confirmed the PSD was off, so we sent them a replacement batch with a tight D90 of 23 microns, and their flooring project went off without a hitch. That’s the kind of detail that makes our job worth it.
If you’re working on a project that requires glass powder, whether it’s a small custom order or a large industrial run, don’t be afraid to ask about PSD testing. Any reputable supplier will be able to share their test methods, their D values, and their lab reports. When we talk to potential clients, we always take the time to walk through how we measure PSD, explain what each number means, and adjust our production process to meet their exact needs—whether that’s a very tight distribution for a high-precision part or a slightly wider distribution for a low-cost, high-volume application.

At the end of the day, measuring particle size distribution for glass powder is a mix of precise science and practical experience. It’s not just about having a fancy laser or a stack of sieves—it’s about taking care with sample prep, running consistent tests, and understanding what those numbers mean for your final product. If you’re tired of batches that don’t perform as expected, or you need custom glass powder with a specific PSD for your next project, don’t hesitate to reach out. We work with clients across industries, from small startups developing new coatings to large manufacturers building industrial filtration systems, and we’re here to make sure you get the right powder, with the right PSD, for your needs.
Zirconia Powder For Sale References
Allen, T. (1997). Particle Size Measurement (5th ed.). Chapman & Hall.
Müller, A. J., & Davy, R. (2009). Dynamic Light Scattering: The Method and Applications. Cambridge University Press.
Society of Tribologists and Lubrication Engineers. (2011). Test Method for Particle Size Distribution of Powders by Sieve Analysis. STLE Standard Test Method STP 522.
Tiantai Leading Technology Co., Ltd.
Tiantai Leading Technology Co., Ltd. is well-known as one of the leading glass powder manufacturers and suppliers in China. Please feel free to buy or wholesale high quality glass powder made in China here from our factory. Contact us for more details.
Address: 4F, 148 Jinpan Road, Tiantai, Zhejiang, 317200, China
E-mail: tzsunflex@qq.com
WebSite: https://www.elecsealing.com/